- Furthermore , we determined the time - to - failure for 70 / 30 ? pldlla cages subjected to loads well below their instantaneous mechanical strength
此外,我们确定了70 / 30聚左旋/消旋乳酸融合器在低于瞬时强度负荷下的衰竭时间。 - Degradable 70 / 30 ? pldlla cages were loaded to failure at loading rates between 10 - 3 and 10 - 1 mm / s under standard loading conditions ( in air at room temperature : 23 )
可降解的70 / 30聚左旋/消旋乳酸融合器载荷直到衰竭,在标准的试验条件下(空气,室温23度)载荷比例为10 - 3和10 - 1 。 - Premature failure of 70 / 30 ? pldlla cages , as observed in vivo in earlier studies , is owing to mechanical loading and the time - dependent mechanical properties of the material
早期的体内观察已经观察到70 / 30聚左旋/消旋乳酸融合器过早的衰竭主要是由于机械负荷和材料本身的时间依靠的机械强度变化。