| 1. | It has been long established that the crimp geometry and crimp properties of synthetic staple fibers decay with the ensuring stages of processing . 长期以来大家一致承认,合成纤维的卷曲形状和性能随着加工阶段的增加而减少。 |
| 2. | Testing method for oil content of synthetic staple fibres 合成短纤维含油率试验方法 |
| 3. | Testing method for defect of synthetic staple fibres 合成短纤维疵点试验方法 |
| 4. | Testing method for length of synthetic staple fibres 合成短纤维长度试验方法 |
| 5. | Testing method for linear density of synthetic staple fibres 合成短纤维线密度试验方法 |
| 6. | Testing method for specific resistance of synthetic staple fibres 合成短纤维比电阻试验方法 |
| 7. | Testing method for crimping performance of synthetic staple fibres 合成短纤维卷曲性能试验方法 |
| 8. | Sampling method of synthetic staple fibres 合成短纤维取样方法 |
| 9. | Testing method for breaking strength and breaking elongation of synthetic staple fibres 合成短纤维断裂强力及断裂伸长试验方法 |