- Crucible 416r should be forged at 2050 to 2150 f ( 1121 to 1177 c ) and finished above 1400 f ( 760 c ) . crucible 416r is not adaptable to severe upset forging operations
在小弟我以前做事的铸造工厂,只要是碰到3字头与4字头铸件变形,都需要热处理后才能整形.要不然内部会产生应力导致铸件破裂 - Abstract : casting for denture restorative trame needs a high quality of equipment , the complex materials , a degree of difficult technique and the useful art . thus it has some difficulty of casting sharpeless and drawbacks ' caused at work . the mutual relations of casting alloy function and casting sprue system inquired , then the measures to solve this casting sharpeless and drawback were provided
文摘:为解决铸造牙科修复支架过程中因各种原因造成铸件变形或缺陷,着重探讨了因铸造合金的性能与浇注系统对铸件的影响,并就解决铸造变形与缺陷提出了相关解决办法。