板的翘曲 - After 20 days at 450 or 1 day at 500 , the u3si2 particles cracked and fragmented , there were a lot of cracks in al - matrix and reacted areas , there were also a lot of holes in the meat . the meat lost its continuity and perfection , and departed from clad . above 450 the volume fraction of the al - matrix and the u3si2 decreased and produced u ( al , si ) 3 in the meat , u3si2 particles invaded to clad
在450热循环20天后、 500热循环1天后,燃料板的厚度变化一般0 . 04mm ,燃料板的翘曲现象严重; u _ 3si _ 2颗粒开裂及破碎,基体中产生大量的裂缝,反应层也存在大量的裂纹及孔洞,芯体已失去连续性、完整性,并且与包壳脱开。