基材厚度 - The results show that , composite could be fabricated on the complicated surface by means of sodium silicate sand mold combination with vacuum infiltration process . when the substrate was 10 mm , composite layers reached 3 mm to 5 mm in thickness with high strength interface and less casting defect . microstructures of grey cast iron and low chromium cast iron matrix composites with various volume fraction has been analyzed
结果表明:用水玻璃砂型(芯)加负压铸渗的工艺能够实现复杂表面(曲面)颗粒增强复合材料的制备,浇注方式简单可靠,基材厚度在10mm时,复合层厚度能达到3 5mm ,且复合层铸造缺陷少,复合效果好,界面致密而且结合强度高。